Iron Octoate Drier 6%
In StockMOQ
25 kg
Lead Time
5–10 days
Packaging
25 kg drums, 200 kg drums
Specifications
| Appearance | Dark amber to brown liquid |
| Flash Point | > 60°C |
| Density (20°C) | 0.93 g/mL |
| Iron Content (Fe) | 6.0% min |
| Viscosity (25°C) | < 50 mPa·s |
FAQ
Iron ions catalyze chromophore formation during oxidative crosslinking, causing perceptible yellowing in the dried film. This limits iron octoate to dark-pigmented systems (deep tones, black, brown). Avoid use in white or light pastel alkyd formulations where color stability is critical.
Interested in Iron Octoate Drier 6%?