Attapulgite Clay Thickener AT-100
CAS 12174-11-7
In StockMOQ
25 kg
Lead Time
5–10 days
Packaging
25 kg bags
Specifications
| Appearance | Off-white to cream powder |
| BET Surface Area | 130–180 m²/g |
| Moisture Content | ≤12% |
| Particle Size (d50) | 5–15 µm |
| pH (5% aqueous dispersion) | 8.0–9.5 |
FAQ
Disperse AT-100 into water or the aqueous phase under high-speed mixing (1000–1500 rpm) for 10–15 minutes before adding binders or pigments. Pre-hydration improves gel network strength by up to 30% compared to post-addition.