Self-Healing Polyurethane Coating Resin SH-200

CAS 9009-54-5

On Request

MOQ

50 kg

Lead Time

10–14 days

Packaging

25 kg drums

Specifications

NV60%
Shore D (cured)45–55
Recovery time at 60°C30 min
Self-healing temperature60°C

FAQ

Self-healing PU uses dynamic disulfide bonds or hindered urea bonds that break and reform under mild heat. At 60°C, chain mobility increases, allowing scratch surfaces to flow together and restore the original surface. Cooling locks in the healed structure.